Corrosion of metals and alloys - Stress corrosion testing - Part 4: Preparation and use of uniaxially loaded tension specimens


Document Number: ISO 7539-4:1989
File Size: 476 kB
Language: English
Provider: ANSI
Shipping: Available for download - Link will be provided in My ComplianceOnline section

Price: $43.00
Product Details

Covers procedures for designing, preparing and using uniaxially loaded tension specimens. These specimens may be used to test a variety of product forms (for example sheet, plate, tubes, wire or rod as well as parts joined by welding, riveting, or other methods). Uniaxially loaded tensile specimens may be stressed quantitatively with equipment for application of either a constant load, a constant strain or an increasing load or strain.