SPECIMEN PREPARATION FOR CROSS DIRECTIONAL INTERNAL TEARING RESISTANCE FOR PAPER, PAPERBOARD AND RELATED MATERIALS
Product Details
Tearing resistance, Cross direction tear, Paper, Paperboard, Nonwovens, Sample preparation
- This practice is used for the preparation of test specimens for the internal tearing resistance of paper, Board, and related materials when a force is applied perpendicular to the machine direction.
- Materials whose structures are highly directional cannot be properly tested in their cross direction according to TAPPI T 414 “Internal Testing Resistance of Paper,” because, as a rule, the tear turns toward the machine direction as it proceeds.
It includes information on:
- Sampling and test specimen
- Conditioning
- Keywords
Customers Also Bought
- Determination of equilibrium moisture in pulp, paper and paperboard for chemical analysis
Price: $53 BUY NOW - Thickness of paper and paperboard (soft platen method)
Price: $53 BUY NOW - Ink rub test of container board and corrugated board
Price: $57 BUY NOW - Edgewise compressive strength of corrugated fiberboard using the clamp method (short column test)
Price: $57 BUY NOW - Indices for whiteness, yellowness, brightness, and luminous reflectance factor
Price: $53 BUY NOW - Coefficient of static friction (slide angle) of packaging and packaging materials (including shipping sack papers, corrugated and solid fiberboard) (inclined plane method)
Price: $57 BUY NOW
You Recently Viewed